Registration Number
0226U000453,
(0125U004213)
, R & D reports
Title
Development of technologies for growing single sapphire crystals and large-block zinc selenide and sulfide crystals for the production of IR transparency windows for special-purpose equipment
popup.stage_title
Розробка технологій вирощування монокристалів сапфіру та крупноблочних кристалів селеніду і сульфіду цинку для виробництва вікон прозорості ІЧ апаратури спеціального призначення, Етап 2025 року
Head
Oleksandr V. Tolmachov, Доктор фізико-математичних наук
Registration Date
09-01-2026
Organization
Institute of Single Crystals of the National Academy of Sciences of Ukraine
popup.description1
improvement of technologies for growing large-sized sapphire single crystals (up to 500 mm×350 mm×20 mm) and large-block optical crystals of zinc selenide and sulfide with a diameter of up to 50 mm and a length of 200 mm
popup.description2
The technological conditions for the growth of large sapphire crystals by the horizontal directed crystallization (HDC) and Stepanov methods were optimized. For the HDC method, the degree of melt overheating from Тm (up to 300 K), temperature gradients along the width (20 K/cm) and length (30 K/cm) of the crystal in the growth zone, the crystallization rate (6-8 mm/h), the parameters of the post-growth cooling stage (two-stage 20 K/h and 40 K/h). For the Stepanov method, the design of the crystal holder and mold was modernized and the temperature gradients along the growth direction were optimized. As a result, sapphire crystals with dimensions of 500 mm × 350 mm × 20 mm (HDC method) and 200 mm × 100 mm × 10 mm (Stepanov method) were obtained, which, in terms of the number of micro- and macrodefects (up to 104 cm-3 and up to 3 cm-3, respectively), correspond to the use of this material in IR optics (optical transmission in the spectral region from 1 μm to 4 μm at the level of 85% at a thickness of 10 mm). Thermal conditions for growth by the Bridgman method under excess argon pressure of ZnSe and ZnS crystals were optimized: the required level of electric power of the heaters, which determines a sufficient temperature level (>1815 K) in the crystallization zone and the program of its change during the ingot growing process with a drawing speed of 1 mm/h, the initial pressure of the inert atmosphere in the middle of the growth chamber (10.5 atm). The ZnSe crystals (50 mm in diameter and up to 150 mm in length) and ZnS (30 mm in diameter and up to 100 mm in length) obtained under the optimized regime are characterized by a low concentration of macrodefects and do not have volume cracking. The obtained large-block (< 4 blocks in volume) ZnSe and ZnS crystals have an optical transmittance of 65-70% (10 mm thick) in the near and mid-IR spectral range from 1.25 μm to 25 μm.
Product Description
popup.authors
Yuliia V. TARANETS
Serhii V. NAIDENOV
Pavlo V. KONEVSЬKYY
Serhii V. NIZHANKOVSKYI
Mykola B. YOLKIN
Oleh O. LUKIYENKO
Oleksii K. KAPUSTNYK
Kateryna P. BURTSEVA
Vitalii L. NADTOCHAYEV
Andrii O. ROMANENKO
Andrii I. HAYDUK
Galyna M. BABENKO
Yuriy T. DYNNYK
Mykola I. MARCHENKO
Oleg A. SMYK
Igor M. DUBTSOV
Vitalii MAKOVIYCHUK
Oleksandr V. TOLMACHOV
Evhenii V. BOCHAROV
Olena I. KOSTENIUKOVA
Andrii I. ENA
Olena M. ERMOLENKO
Olena M. NAUMENKO
Yurii A. LUBCHICH
Oleksandr Y. SERDYUK
Evhenii V. SLYUNIN
Oleksandr T. BUDNIKOV
Bohdan Y. KUTS
Inna A. EFYMENKO
Dmytro S. SOFRONOV
Oleksandr V. VOLOSHYN
Leonid O. HRYN
Serhii I. KRYVONOHOV
Olena F. DOLZHENKOVA
Yurii V. BARYLOV
Volodymyr F. BOCHKOV
Alla K. PESETSKA
popup.nrat_date
2026-01-09